Ubuncinane boMyinge weodolo:Iikhilogram ezili-100
Iinkcukacha zokuPakisha:
Pack A: 16kg / Metal umphanda
Iipakethi B: 24KG iPlasitiki yomphanda
Ipakethe C:Isekwe kwisixa se-arhente A
Ixesha lokuzisa:Kwiintsuku ezilishumi emva kokufumana intlawulo kwangaphambili
Ubunakho bokubonelela:Iitoni ezi-2 ngosuku
Indlela yokwaleka:Dip Spin & Spray
Umbala:Isilivere
PH:3.8-5.2
Ubunzima obuthile:1.33±0.05( Ukutshiza)1.33±0.05(iDip-spin Coating)
Viscosity:NgokweMfuno yokuSebenza.
Ubushushu bokusebenza:20±2℃
Inkcazo
I-JH-9382 yenziwe ngeepakethe ezintathu: A,B noC;
Ipakethe A: Yisilivere engwevu ludaka oludityaniswe ikakhulu ngokwekhemikhali kunye neflake entle kakhulu iZn, iflake entle kakhulu iAl kunye nesongezo sendalo.
I-Pack B: Sisisombululo samanzi esidityaniswe ikakhulu kunye ne-corrosion protecion additive, isisombululo esithile samanzi esilawulayo njl.
Ipakethe C: Yeyona nto ibambekayo yokwaleka eyenziwe ikakhulu ngeselulosi emhlophe okanye ngumgubo omthubi.
Iimpawu zokusebenza:
Ifilimu imhlophe yesilivere, ukugqiba kakuhle komphezulu, ukuxhathisa okuphezulu kwe-corrosion, ukugquma okulungileyo.
Inkqubo yokwaleka
1. Mix Ratio
Pack A: 16.0 kg
Ipakethe B:24.0 kg (ubungakanani bunokwandiswa ngokufanelekileyo ukuba kugqunywe isitshizi)
Iipakethi C: 0-50 g (ngokwemfuno ye-viscosity eyahlukeneyo)
2. Phambi koMxube, Gcina ii-A&B ezinobunzima kubhafu wamanzi nge-25±2℃, emva koko uvuthulule u-A ukwenza uludaka lwesinyithi lusasazeke ngokufanayo ngomxube ophindaphindayo, emva kokuba u-A esasazwe ngokulinganayo, nciphisa isantya esiphazamisayo ukuya ku-60r/min, kwaye wongeze i-B. .
Yongeza u-B ku-A ngokukhawuleza.Okwangoku, iqondo lobushushu lomgqomo liya kunyuka, xa lifikelela kuma-35 ℃, qalisa isixhobo sokukhenkceza ukugcina iqondo lobushushu lomgqomo lingaguquki kwi-35 ℃.
3.Yongeza u-B ku-A ngokukhawuleza.Okwangoku, iqondo lobushushu lomphanda liya kunyuka, xa lifikelela kuma-35 ℃, isixhobo sokuqalisa sokukhenkceza ukugcina iqondo lobushushu lomphanda lingaguquki kuma-35 ℃.
4. Gxuma umxube malunga neyure ezi-1 ~ 2 ngokukhawuleza emva kokuba i-B ifakiwe, uze udibanise i-C. C kufuneka ibe ngumgubo ukuba kukho iqhuma. Iiyure ezili-12 ngokuqhubekayo.
5. Ukwaleka kufuneka kuhluzwe nge-100 ye-mesh stainless steel screen phambi kokuba igalelwe kwidip barrel.
6. Isixhobo sokulawula ubushushu kufuneka sixhotyiswe ngediphu yombhobho ukugcina ubushushu bokugquma kwi-22±2℃.
(Ukuba i-temp. iphezulu kakhulu, ipeyinti inoxanduva lokuwohloka, kwaye i-viscosity iya kwenziwa.) I-coating kufuneka ixutywe ngesetyhula ukuze igcinwe ngokulinganayo.
7. Ubuninzi bovavanyo, i-PH, iTemperature, i-Viscosity kunye ne-Cr6 + umxholo wokugquma zonke iiyure ze-8 ukuba zisebenza ngokuqhubekayo.
Xuba uMzobo
Ukuqwalaselwa
Ezinye iikhemikhali ezinjengazo naziphi na iintlobo ze-asidi, ityuwa yealkali ayinakuxutywa kwi-coating, kuba ezi zinokuvula i-Zn kunye ne-Al plate ukuze iguge isambatho.
Gwema ukukhanya kwelanga kunye ne-ultraviolet ray ixesha elide xa usebenza, ngaphandle koko kuya kukhawulezisa ukuguga okanye i-polymerization yokwambathisa.
Kubaluleke kakhulu ukulawula ukushisa kwengubo.Ukuba iqondo lobushushu bokwambathisa liyatshintsha xa usebenza, liya kusebenzisa i-viscosity, emva koko i-effec i-quatity yokwambathisa kwi-workpiece.Ke ubudlelwane phakathi kobushushu, i-viscosity kunye nenkqubo yokusonta kufuneka ilawulwe kakuhle xa kugqunywa.
I-viscosity iya kuhluka ukuba indlela yokugqoka iyahluka.Khetha idata esezantsi ukuba isitshizi ityabeka, kwaye ukhethe idatha ephezulu ukuba dip spin coating.
Idatha yoBugcisa
Hayi. | Into | Idatha |
1 | Umbala | Isilivere |
2 | Indlela yokwaleka | Dip Spin & Ukutshiza |
3 | PH | 3.8-5.2 |
4 | Cr6+ | ≥25g/L |
5 | Ubunzima obuthile | 1.33±0.05(ukutshiza)1.33±0.05(i-dip-spin coating) |
6 | Viscosity | Ngokwemfuno yokusebenza. |
7 | Ubushushu bokusebenza | 20±2℃ |