ibhanile-imveliso

Chrome Free Zinc Flake Coating JH-9610

Inkcazelo emfutshane:

Igama lebrand:JUNHE

Inombolo yoMfanekiso:JH-9610


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ubuncinane boMyinge weodolo:100 Kiloam
Iinkcukacha zokuPakisha:
Pack A: 20kg / Metal umphanda
Iipakethi B: 20KG iPlastiki yomphanda
Ipakethe C:Isekwe kwisixa se-arhente A
Ixesha lokuzisa:Kwiintsuku ezilishumi emva kokufumana intlawulo kwangaphambili
Immimiselo yokuhlawula:L/C, T/T
Ubunakho bokubonelela:Iitoni ezi-2/iiToni ngosuku

Umbala:Isilivere
Indlela yokwaleka:Dip kwaye utshize ukutyabeka
PH(20℃):5.0-8.0
Ubunzima obuthile:1.30-1.40 (ukutshiza iCoating)
Viscosity:Ngokutsho kweMfuno yokuSebenza
Ubushushu bokusebenza:22±2℃

Inkcazo

I-JH-9610 yenziwe ngeepakethe ezintathu: A,B noC;
Ipakethe A: Yisilivere engwevu ludaka oludityaniswe ikakhulu ngokwekhemikhali kunye neflake entle kakhulu iZn, iflake entle kakhulu iAl kunye nesongezo sendalo.
I-Pack B: Sisisombululo samanzi esidityaniswe ikakhulu kunye ne-corrosion protecion additive, isisombululo esithile samanzi esilawulayo njl.
Ipakethe C: Yeyona nto ibambekayo yokwaleka eyenziwe ikakhulu ngeselulosi emhlophe okanye ngumgubo omthubi.

Iimpawu zokuSebenza:
1. IChrome yasimahla;
2. Ukusebenza kakuhle komphezulu wokugqibezela, ukuchasana nomhlwa okuphezulu, umlinganiso ophantsi wokukhuhlana;
3. Akukho brittleness hydrogen, akukho nkqubo pickling;
4. Ukumelana nobushushu obuhle;
5. Iiyure ze-SST ezilungileyo, umjikelo wokulwa nokuguga ude, unokugqoka iimveliso ezininzi phantsi kweemeko zenkqubo efanayo.

Inkqubo yokwaleka

1. Mix Ratio
Ipakethe A: Ipakethe B: Ipakethe C=1:1: X(ngokwemfuno ye-viscosity eyahlukileyo)

2. Phambi koMxube, Gcina ii-A&B ezinobunzima kubhafu wamanzi nge-25±2℃, emva koko uvuthulule u-A ukwenza uludaka lwesinyithi lusasazeke ngokufanayo ngomxube ophindaphindayo, emva kokuba u-A esasazwe ngokulinganayo, nciphisa isantya esiphazamisayo ukuya ku-60r/min, kwaye wongeze i-B. .

3. Yongeza u-B ku-A ngokukhawuleza.

4. Gxuma umxube malunga neeyure ezi-1 ~ 2 emva kokuba i-B ifakiwe, uze udibanise i-C. C kufuneka ibe ngumgubo ukuba kukho iqhuma. ~iiyure ezili-12 ziphantsi kwaye ngokuqhubekayo.

ukutyabeka

Xuba uMzobo

xuba

Ukuqwalaselwa

1. Ezinye iikhemikhali ezifana naluphi na uhlobo lwe-asidi, ityuwa ye-alkali ayinakuxutywa kwi-coating, kuba ezi zingenza i-Zn & Al plate isebenze ukuguga kwengubo.

2. Gwema ukukhanya kwelanga kunye ne-ultraviolet ray ixesha elide xa usebenza, ngaphandle koko kuya kukhawuleza ukuguga okanye i-polymerization yengubo.

3. Kubaluleke kakhulu ukulawula ukushisa kwengubo.Ukuba iqondo lobushushu bokwambathisa liyatshintsha xa usebenza, liya kusebenzisa i-viscosity, emva koko i-effec i-quatity yokwambathisa kwi-workpiece.Ke ubudlelwane phakathi kobushushu, i-viscosity kunye nenkqubo yokusonta kufuneka ilawulwe kakuhle xa uqatywa.

4. I-viscosity iya kuhluka ukuba indlela yokugqoka iyahluka.Khetha idata esezantsi ukuba isitshizi ityabeka, kwaye ukhethe idatha ephezulu ukuba dip spin coating.

Idatha yoBugcisa

Hayi. Into Idatha
1 Umbala Isilivere
2 Indlela yokwaleka Ukuntywila kunye nokutshiza
3 PH 4.8-7.5
4 Ubunzima obuthile 1.45±0.1(iNgqungquthela yokutshiza)
5 Viscosity 25 ~ 40s(Ukutshiza)

  • Ngaphambili:
  • Okulandelayo:

  • Bhala umyalezo wakho apha kwaye uwuthumele kuthi